Uns S17400 of AMS5604 Hot Rolled Sheet Age
Overview .lc-a-img { position: relative; width: 100%; height: 100%; object-fit: contain; overflow: hidden;}.lc-a-img .im
- Overview
- Product Description
- Equivalent Grades Standards
- Chemical composition
- Typical delivery condition & mechanical properties
- FAQ
Basic Info.
| Model NO. | uns s17400/630/1.4542/17-4ph/0Cr17Ni4Cu4Nb/ |
| Grade | 600 Series |
| Certification | ISO, Gjb |
| Shape | Flat |
| Technique | Hot Rolled |
| Surface Treatment | Polished |
| Heat Treatment | Solution or Age-Hardening |
| Surface | Black or 1e Polished to Bright |
| Width | ≤2200mm |
| Length | Limited or Random |
| NDT | 100% Ut |
| Transport Package | as Required |
| Specification | thickness 8-120mm |
| Trademark | SMTCO |
| Origin | China |
| HS Code | 7219210000 |
| Production Capacity | 5000t Per Year |
Product Description
Product DescriptionIntroductionThis martensitic precipitation-hardened stainless steel, enhanced with copper and niobium, builds upon the 0Cr15Ni5Cu4Nb base alloy and further optimizes its chemical composition and overall performance. Through the synergistic strengthening effects of copper and niobium, combined with precisely controlled heat treatment processes, this steel achieves a superior combination of mechanical properties compared to conventional martensitic stainless steels. It exhibits excellent tensile strength along with good ductility and toughness, making it an ideal choice for critical load-bearing structures. In terms of corrosion resistance, this steel significantly outperforms traditional martensitic stainless steels such as Cr13, 9Cr18, and 1Cr17Ni2. The synergistic effect of chromium, copper, and niobium endows it with enhanced resistance to pitting and crevice corrosion in chloride environments, particularly reaching its optimal corrosion resistance when aged at H1150. This steel also excels in corrosion fatigue performance; experimental data show that its corrosion fatigue limit is more than 30% higher than that of 12%Cr martensitic steels, and its resistance to water droplet erosion has been markedly improved as well. Regarding fabrication processes, this steel demonstrates excellent weldability and can be joined using conventional methods such as shielded metal arc welding and laser welding. After welding, its properties can be readily restored through simple post-weld heat treatment. It boasts outstanding forging characteristics, with a wide range of hot-working temperatures; however, its cold-forming capabilities are relatively limited. For parts with complex geometries, it is recommended to employ hot-forming processes.ApplicationsIn the aerospace industry, this material is widely used to manufacture critical load-bearing structural components of aircraft, including landing gear parts, engine mounting brackets, actuators for flight control systems, and high-strength fasteners for spacecraft. In the energy equipment sector, it is an ideal choice for gas turbine compressor blades, main pump shafts and valve components in nuclear power plants. In the petrochemical industry, it is primarily employed in critical equipment operating in highly corrosive environments—for example, valve bodies for deep-sea oil production trees, impellers and shaft sleeves for chemical process pumps. In the marine engineering field, it is commonly used to fabricate high-pressure pump components for seawater desalination units, hydraulic system components for submarines, and fastening and connecting elements for offshore platforms. Additionally, in the high-end equipment manufacturing sector, it can also be utilized in the production of precision molds, medical devices (such as orthopedic surgical instruments), and key components for defense industry products.Equivalent Grades Standards| Steel Grade | Specification | Specification Name |
| 0Cr17Ni4Cu4Nb / 05Cr17Ni4Cu4Nb / S51740 | GB/T 1220 | Stainless steel bars |
| GB/T 1221 | Heat-resistant steel bar | |
| GB/T 8732 | Steels of blade for steam turbine | |
| GB/T 4238 | Heat-resisting steel plate, sheet and strip | |
| GJB 8268 | Specification for precipitation-hardening stainless steel bars for aviation | |
| UNS S17400 / 630/1.4548/1.4542 | ASTM A564/A564M | Standard Specification for Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes |
| ASTM A693 | Standard Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip | |
| AMS 5604 | 16.5Cr-4.0Ni-4.0Cu-0.30Cb Aerospace material Specification-Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr-4.0Ni-4.0Cu-0.30Cb Solution Heat Treated, Precipitation Hardenable | |
| AMS 5643 | 16Cr-4.0Ni-0.30Cb(Nb)-4.0Cu Aerospace material Specification-Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr-4.0Ni-0.30Cb(Nb)-4.0Cu Solution Heat Treated, Precipitation Hardenable | |
| AMS 5622 | 16Cr-4.0Ni-0.30Cb(Nb)-4.0Cu Aerospace material Specification-Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr-4.0Ni-0.30Cb(Nb)-4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted | |
| 1.4542 / X5CrNiCuNb16-4 | EN 10088-3 | Stainless Steels Part 3-Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes |
| X5CrNiCuNb16-4 | ISO 683-18 | Stainless steels for general purposes – Part 1: Corrosion-resistant flat products |
| SUS630 | JIS G 4303 | Stainless Steel bars |
| JIS G 4304 | Hot rolled stainless steel sheet and strip | |
| JIS G 4305 | Cold rolled stainless steel sheet and strip | |
| JIS G 4308 | Stainless steel wire rods | |
| Remark: Products produced as per other specifications or technical agreements (if need) are available. | ||
| Elements | C | Si | Mn | P | S | Ni | Cr | Cu | Nb |
| Content% | ≤0.07 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.030 | 3.00~5.00 | 15.00~17.50 | 3.00~5.00 | 0.15~0.45 |
| Remark: Products produced as per other specifications or technical agreements (if need) are available. | |||||||||
| Delivery Condition | Mechanical Properties | ||||||
| Rp0.2 (N/mm2) | Rm (N/mm2) | A/% | Zb/% | Akv2d/J | HBW | HRC | |
| Cond. A 1040℃±15℃ | / | / | / | / | / | ≤363 | ≤38 |
| H900, 480℃, 1h, air | ≥1170 | ≥1310 | ≥10 | ≥40 | / | ≥388 | ≥40 |
| H925, 495℃, 4h, air | ≥1070 | ≥1170 | ≥10 | ≥44 | ≥6.8 | ≥375 | ≥38 |
| H1025, 550℃, 4h, air | ≥1000 | ≥1070 | ≥12 | ≥45 | ≥20 | ≥331 | ≥35 |
| H1075, 580℃, 4h, air | ≥860 | ≥1000 | ≥13 | ≥45 | ≥27 | ≥311 | ≥32 |
| H1100, 595℃, 4h, air | ≥795 | ≥965 | ≥14 | ≥45 | ≥34 | ≥302 | ≥31 |
| H1150, 620℃, 4h, air | ≥725 | ≥930 | ≥16 | ≥50 | ≥41 | ≥277 | ≥28 |
| H1150M, 760℃, 2h, air; 620℃, 4h, air | ≥520 | ≥795 | ≥18 | ≥55 | ≥75 | ≥255 | ≥24 |
| H1150D, 620℃, 4h, air; 620℃, 4h, air | ≥725 | ≥860 | ≥16 | ≥50 | ≥41 | 255~311 | 24~33 |
| Remark: Products produced as per other specifications or technical agreements (if need) are available. | |||||||
Send to us